On a galvanised sheet the number after the Z is the part worth paying for. Z275 means about 275 grams of zinc per square metre, counted over both faces together. Zinc wears away slowly and protects the steel even at small scratches, so in a given climate the life of the sheet rises roughly with that coat mass. The same steel is sold as flat sheet for fabrication and as profiled roof sheet.
Price guide
Steel merchants list flat galvanised sheets of 2450 x 1225 mm at about R350 to R397 for 0.5 mm and about R755 to R764 for 1.2 mm, incl. VAT on two of the three lists.
A rough guide from published South African prices. Thickness, coating, length, cutting, delivery and VAT all move it.
What do the coat classes mean in practice?
| Class | Commonly used for |
|---|---|
| Z100 and lighter | Dry indoor work, ducts above ceilings |
| Z200 | General fabrication, sheltered outdoor parts |
| Z275 | Roofing, gutters, outdoor work |
| Z450 to Z600 | Harsher sites, longer life |
Site matters as much as class. A sheet that lasts decades on a dry Free State farm may show rust far sooner at the coast or near a smelter. Parts made from bare steel and then dipped after fabrication get a much thicker coat; ask a fabricator about hot dip galvanising.
Flat sheet or profiled sheet?
Flat galvanised sheet commonly comes in 1225 x 2450 mm and 1250 x 2500 mm sizes, in coil and as slit strip, from about 0.5 mm up to around 3 mm. Fabricators fold it into ducting, gutters, downpipes, flashings, brackets, cable trays and feed troughs. Profiled galvanised roof sheet is the plain, unpainted budget option for sheds. Old drawings often give thickness in gauge: the gauge converter turns that into millimetres, and the weight calculator gives the mass.
Is it safe to weld or cut galvanised steel?
With care. Heat turns the zinc into fumes that can cause metal fume fever, a flu like illness. Weld in moving air with extraction and a suitable respirator, never in a closed room, and grind the coat back from the joint first. Paint the finished weld with a zinc rich paint to restore protection.
What is the white powder on my new sheets?
White rust. When stacked sheets get wet, the trapped water attacks the zinc and leaves a white, chalky deposit. Keep the pack raised on timber, sloped a little so water runs off, under a tarpaulin with gaps for air, and separate any sheets that got wet so they dry. Ask for passivated sheet, which resists it better. A light bloom usually weathers away once the sheets are fixed; heavy deposits with dark grey patches underneath mean the coat has been eaten.
Who asks for this
- Homeowners and DIY
- A shed roof, a gutter repair or a flashing folded to close a gap above a window.
- Builders and contractors
- Flashings, lintel trays and duct sections bought flat and folded on site.
- Farms and smallholdings
- Feed troughs, chicken houses and plain roofs over sheds where cost leads.
- Factories and workshops
- Ducting, machine covers, brackets and cable trays made in the sheet metal shop.
- Shopfitters and signwriters
- Extraction hoods and duct runs in restaurant kitchens before the stainless trim goes on.
- Schools, clinics and municipalities
- Ventilation ducting in schools and hospitals and repairs to old outbuilding roofs.
- Mines and plants
- Ventilation ducting and guards, often in heavier coat classes for wet conditions.
- Resellers, fabricators and installers
- HVAC installers and sheet metal workers buying full sheets and coils in bulk.
Frequently asked questions
Is galvanised the same as zinc or Zincalume sheet?
Galvanised is a pure zinc coat. Aluminium zinc is a different coat that commonly lasts longer in sun and salt air; the zinc sheets page compares them.
Can galvanised sheet touch copper?
Keep them apart. Copper pipes, and even water dripping from a copper geyser overflow, pit the zinc quickly. Lead flashings and bare steel cause the same problem.
Can I paint galvanised sheet?
Yes, with a primer made for galvanised surfaces, or after the shine has weathered off. Ordinary enamel straight onto new galvanising tends to peel within a season or two, so degrease the sheet and follow the paint maker's system for metal.
What is the spangle on the surface?
The pattern of zinc crystals formed as the coat cools. Sheet meant for painting is often made with a minimised spangle for a smoother finish.